    Default Bathrooms / high humidity


    Hi guys,
    What does everyone else use to tape bathrooms and areas with high humidity. I have been using Lafarge aquamix but can't always get hold of it so was wondering if there are other ways.
    Cheers.

  2. #2
    Getting the hang of this Captain perfect's Avatar
    Join Date
    May 2009
    Location
    West Sussex
    Posts
    173
    Thanks
    7
    Thanked 15 Times in 14 Posts

    Default

    Gypsum red filler & two coats of BG Quicksand for me,




    & Welcome
    Milk No Sugar.

  3. #3
    VIP TonyM's Avatar
    Join Date
    Jan 2009
    Posts
    1,330
    Thanks
    52
    Thanked 187 Times in 160 Posts

    Default

    I'm using Aquamix on Aquapanel at the moment and I don't like how it shrinks after a couple of days. Get it no problem from Encon or Minsters.

  4. #4
    Newbie
    Join Date
    Mar 2012
    Posts
    2
    Thanks
    0
    Thanked 0 Times in 0 Posts

    Default

    Thanks for the replies. Talked to a guy a while ago who used scrim, easi fill and smart mix top coat, claimed to never have had a problem and quick but putting scrim in corners does not appeal much.

  5. #5
    Member
    Join Date
    Aug 2011
    Location
    UK OXON
    Posts
    63
    Thanks
    18
    Thanked 3 Times in 3 Posts

    Default

    Quote Originally Posted by Captain perfect View Post
    Gypsum red filler & two coats of BG Quicksand for me,




    & Welcome
    same here
    Taping & jointing
    Phone : 07526 221905

  6. #6
    Season Ticket Holder DMC's Avatar
    Join Date
    May 2010
    Location
    SCOTLAND
    Posts
    522
    Thanks
    22
    Thanked 74 Times in 68 Posts

    Default

    Quote Originally Posted by Captain perfect View Post
    Gypsum red filler & two coats of BG Quicksand for me,
    Works for me

  7. #7
    VIP E.K Taper's Avatar
    Join Date
    May 2010
    Location
    East Kilbride, Glasgow
    Posts
    1,385
    Thanks
    386
    Thanked 199 Times in 177 Posts

    Default

    Quote Originally Posted by Captain perfect View Post
    Gypsum red filler & two coats of BG Quicksand for me,
    And me!!!

  8. #8
    Season Ticket Holder scottishlad2k10's Avatar
    Join Date
    Sep 2010
    Location
    scotland
    Posts
    548
    Thanks
    23
    Thanked 21 Times in 21 Posts

    Default

    i didnt realise/know you were supposed to use anything different? its always just the fast set bg and readymix pro. 2 coats fast set 1 finish, couple of coats of universal primer(expencive but worth it in the long run) . followed by couple of coats of softsheen or bathroom paint never had any problems? but regulations now make you fit an extractor of some sort?

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

Similar Threads

  1. High Stepper Stilts
    By Brian S in forum Taping tools and materials
    Replies: 4
    Last Post: 13-08-2011, 07:10 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •